Steel plate boiler specialmaterials zinc are low Si, low C, with a suitable amount ofMn, steel construction can
welding. The zinc kettle can fight the collision of zinc, and can withstand high temperature.
The chemical components are:
Components |
C |
Si |
Mn |
P |
S |
AL |
Max% |
0.08 |
0.02 |
0.50 |
0.015 |
0.010 |
0.040 |
Practical number |
0.047 |
0.003 |
0.42 |
0.008 |
0.0058 |
0.024 |
The zinc kettle life is decided by the iron loss is related to the loss of iron zinc boiler temperature and life
boiler zinc:
438 ° C: 14;years
450 ° C: 10;years
460 ° C: 8years;
480 ° C: 6;years
490 ° C: 4.3 years;
495 ° C: 2.9 years;
We are professional manufacturer for galvanizing kettle, can provide high quality product for you, welcome inquiry.